Solid-phase extraction and separation of indium with P2O4-UiO-66-MOFs (di-2-ethylhexyl phosphoric acid-UiO-66-metal-organic frameworks)


Minglai Fu , Wan-Yi Zeng , Minzhong Huang

DOI:10.1016/j.jes.2022.08.003

Received May 03, 2022,Revised , Accepted August 01, 2022, Available online August 09, 2022

Volume 35,2023,Pages 833-843

Compared with the traditional liquid–liquid extraction method, solid-phase extraction agents are of great significance for the recovery of indium metal due to their convenience, free of organic solvents, and fully exposed activity. In this study, P2O4 (di-2-ethylhexyl phosphoric acid) was chemically modified by using UiO-66 to form the solid-phase extraction agent P2O4-UiO-66-MOFs (di-2-ethylhexyl phosphoric acid-UiO-66-metal-organic frameworks) to adsorb In(III). The results show that the Zr of UiO-66 bonds with the P-OH of P2O4 to form a composite P2O4-UiO-66-MOF, which was confirmed by X-ray photoelectron spectroscopy (XPS) and Fourier transform infrared spectroscopy (FT-IR). The adsorption process of indium on P2O4-UiO-66-MOFs followed pseudo first-order kinetics, and the adsorption isotherms fit the Langmuir adsorption isotherm model. The adsorption capabilities can reach 192.8 mg/g. After five consecutive cycles of adsorption-desorption-regeneration, the indium adsorption capacity by P2O4-UiO-66-MOFs remained above 99%. The adsorption mechanism analysis showed that the P=O and P-OH of P2O4 molecules coated on the surface of P2O4-UiO-66-MOFs participated in the adsorption reaction of indium. In this paper, the extractant P2O4 was modified into solid P2O4-UiO-66-MOFs for the first time. This work provides a new idea for the development of solid-phase extractants for the recovery of indium.

Copyright © Research Center for Eco-Environmental Sciences, Chinese Academy of Sciences. Published by Elsevier B.V. and Science Press. All rights reserved.京ICP备05002858号-3